Feritne RM jezgre

Feritne RM jezgre

 

product-553-317
product-553-317

Model

G.W

VELIČINA (mm)

A1

A

B

C

D

E

F

Gmin

H

RM6

5.6

14.4±0.3

17.55±0.35

12.65±0.25

8.0±0.2

6.3±0.1

4.1±0.1

8.8±0.1

8.8

10.3±0.3

RM8

13.6

19.3±0.4

22.7±0.5

17.3±0.3

10.7±0.3

8.4±0.2

5.5±0.1

11.4±0.5

9.5

14.3±0.3

RM10

24

24.1±0.6

27.8±0.7

21.6±0.5

13.2±0.3

10.7±0.2

6.3±0.2

9.3±0.1

10.9

16.2±0.3

RM12

49

29.2±0.6

36.7±0.7

25.5±0.5

15.8±0.3

12.6±0.2

8.5±0.2

11.85±0.1

16.8

21.6±0.3

RM14

77

34.1±0.6

41.5±0.7

29.6±0.6

18.7±0.3

14.7±0.3

10.6±0.1

15.5±0.1

17.0

27.0±0.3

 

MODEL

PARAMETAR

AL±25%(nH/N^2)

N.W(g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

ZH7K

ZH10K

RM6

0.784

29.2

37.0

1090.0

2150

6000

8600

4.9

RM8

0.604

38.4

63.0

2440.0

3300

8750

12500

12.0

RM10

0.462

44.6

96.6

43100.0

4000

11200

16000

22.0

RM12

0.388

56.6

146.0

8340.0

5000

13000

17700

45.0

RM14

0.35

70

198.0

13900.0

5700

14500

19600

67.0

Popularni tagovi: feritne rm jezgre, proizvođači, dobavljači, tvornica feritnih rm jezgri u Kini